LIC LZC Niobium Tantalum Based Halide Solid Electrolyte For Solid State Battery Materials Research

​​Model:LIC/LZC
​​​​​​Ionic Conductivity​​​​​:1.2–2.5 mS/cm ​
Electrochemical Window​​​​:1.5–4.3 V ​​Density​​​​:2.8 g/cm³
​​​​​Moisture Sensitivity​:High
​​Processing​​​:Ball-mill for 10h (Zr-based) or sol-gel synthesis for Ta/Nb systems.
​Storage:Argon-filled glovebox (O₂/H₂O <0.1 ppm) for LIC; dry air (<30% RH) for LZC.
Temperature​​:25°C
MOQ: 10g
Leading time: 5-7 working days

Li10GeP2S12 Lithium Battery Solid State Electrolyte LGPS Ceramic Electrolyte 1-5um

​​Model:Li10GeP2S12
​​Crystal Structure​​​​​​:Tetragonal (P4₂/nmc) ​
Particle Size​:1-5 μm (laser verified)
​​​​Ionic Conductivity​​​​​:12 mS/cm @25°C (highest among sulfides)
​​​​​Electrochemical Window​:0-5V vs. Li⁺/Li
​​​​Density​​​​:2.14 g/cm³
​​Storage:Dry environment (desiccator recommended)
Temperature​​:25°C
MOQ: 10g
Leading time: 5-7 working days

Li6PS5Cl LPSCl Lithium Ion Battery Solid Electrolyte Powder 1-5um For Scientific Research

​​Model:Li₆PS₅Cl
​​​Particle Size​​​​​​​:1-5 μm ​
​​Ionic Conductivity​​:~10⁻³ S/cm (25°C)
Bulk Resistance​:127 Ω (300MPa pressed)
​​Pellet Density​​:1670 μm thickness
​​​​Handling Requirements​​​​​:Argon glovebox
​​​Storage:Dry environment (desiccator recommended)
Temperature​​:25°C
MOQ: 10g
Leading time: 5-7 working days

Li1.5Al0.5Ge1.5(PO4)3 LAGP Lithium Aluminum Germanium Phosphate Solid Electrolyte Powder 1-5um

​​Model:Li₁.₅Al₀.₅Ge₁.₅(PO₄)₃
​​​​​Appearance​:Pure white powder ​
​​Ionic Conductivity​​​:4×10⁻⁴ S/cm (25°C)
Particle Size (D50)​​:1-5 μm
​​Packaging​​​:10g glass bottle
​​​​Applications​​​​​​:Solid-state lithium batteries
​​​Storage:Dry environment (recommended); short-term air exposure permissible
Temperature​​:25°C
MOQ: 10g
Leading time: 5-7 working days

Li2S All Solid State Battery Raw Materials Anhydrous High Purity Lithium Sulfide

​​Model:Li2S
​​​​​Test Standard​​:GB/T 11064 ​
​​​​Purity​:≥99.9% (4N grade)
​Crystal Structure​:Cubic (anti-fluorite)
​​Melting Point​​​​:938°C
​​​​​​Density​​​​​​​:1.66 g/cm³
​​​​​Particle Size​:D50 ≤5 μm (customizable)
​​Moisture Sensitivity​:<0.1 ppm H₂O (Ar-sealed)
MOQ: 10g
Leading time: 5-7 working days

Lithium Aluminum Titanium Phosphate LATP Nasicon Oxide Solid Ceramic Electrolyte Powder

​​Model:Li₁.₅Al₀.₃Ti₁.₇(PO₄)₃
​​​​​Particle Size​​​:300 nm – 5 μm (multiple grades) ​
​​​​Purity​:≥99.9% (4N grade)
​​​Ionic Conductivity​​:2–5×10⁻⁴ S/cm (25°C)
​​Packaging​:10 g, 50 g, 100 g/bottle
​​​​​​​​Li Content​​​​​​​​:41.3 wt% (theoretical)
MOQ: 10g
Leading time: 5-7 working days

2.3 Sodium Iron Pyrophosphate NFPP Sodium Ion Battery Cathode Material

​​Model:NFPP
Chemical Formula​​​​:Na₄Fe₃(PO₄)₂P₂O₇​
​​​​Purity​:≥99.9% (4N grade)
Tap Density​​​:2.3 ± 0.1 g/cm³
article Size (D50)​​:6–12 μm
​​​​​​​​​​Specific Surface Area​:≤10 m²/g
​​​​​​​​​​​​0.1C Capacity​​:≥105 mAh/g
​​1C Capacity​​​:≥95 mAh/g
MOQ: 10g
Leading time: 5-7 working days

4N Solid State Battery Materials High Purity Titanium Hydride TiH2 Powder

​​Model:TiH2
​​​​Purity​:≥99.99% (4N)
​​​​Particle Size (D50)​:Customizable (1-50 µm)
​​Density​​​​:3.76–4.26 g/cm³
​​Appearance​:Gray-black powder
​​​​​​​​​​​​Moisture Content​​:≤100 ppm
​​​​​​​​​​​​Oxygen Content​​​:0.01%
​​Hydrogen Release Temp:400–1000°C (adjustable)
MOQ: 10g
Leading time: 5-7 working days

LiCl Lithium Chloride Anhydrous Lithium Salt For Solid Electrolyte Lithium Battery

​​Model:LiCl
​​​​​Appearance​​:White crystalline granules
​​​​Density​​:2.068 g/cm³
​​​​Melting Point​​​​​:605°C
​​Purity​:99%
​​​​​​​​​​​​Molecular Weight​​:42.39
​​​​​​​​​​​​Applications​​​:1. Lithium salt for battery cathodes/solid electrolytes 2. Metallic lithium production
​​Storage Conditions:Sealed, low-humidity environment
MOQ: 10g
Leading time: 5-7 working days

Niobium Containing LLZTO Solid Electrolyte Tantalum Niobium Co Doped Lithium Lanthanum Zirconium Oxygen 500nm

​​Cycle life:500-1000 cycles
​​​​​Capacity​​:Typically 3.6V and 1000mAh/g
​​​​Disposal​​:Requires special disposal methods due to toxic materials
​​​​Weight:Lightweight compared to other battery types
Energy density​:Up to 200 Wh/kg
​​​​​​​​​​​​Safety​​:Highly flammable and sensitive to temperature
​​​​​​​​​​​​Self-discharge rate​​​:1-2% per month
​​Operating temperature:-20°C to 60°C
MOQ: 10g
Leading time: 5-7 working days

LATP Lithium Aluminum Titanium Phosphate Solid Electrolyte Sheet Li1.3Al0.3Ti1.7 PO4

​​Model:Li₁.₃Al₀.₃Ti₁.₇(PO₄)₃
​​​​​​​Dimensions​:13×1mm (stock), 6.8×1mm
​​​​​​Density​​​:2.77 g/cm³ (94% theoretical)
Ionic Conductivity​:0.7 mS/cm @25°C
​​Lead Time​​:In stock (13mm), 1 week (6.8mm)
​​​​​​​​​​​​Applications​:​​All-Solid-State Batteries
​​​​​​​​​​​​​Storage​​​:Dry environment (desiccator recommended)
​​Temperature:25°C
MOQ: 10g
Leading time: 5-7 working days

LLZTO Solid Electrolyte Tantalum Doped Lithium Lanthanum Zirconium Oxygen Li6.5La3Zr1.5Ta0.5O12

​​Model:LLZTO
​​​​​​​Crystal Structure​:Cubic garnet (Ia-3d)
​​​​​​Density​​​:95% theoretical (5.1 g/cm³)
Thickness Options​​:50–300 μm (customizable)
​​Ionic Conductivity​:1.68×10 −3 S/cm (25°C)
​​Activation Energy​:​​0.25–0.30 eV
Thermal Stability​:Up to 1000°C (melting point)
​​Storage:Argon glovebox (O₂/H₂O <0.1 ppm) to prevent Li₂CO₃ formation
MOQ:10pcs
Leading time: 5-7 working days

Porous Silicon-Carbon Anode Material Si/C for Lithium-Ion Batteries with High Capacity and Long Cycle Life

​​Model:SiC
​​​​​​​Specific Surface Area​:≤8.0m²/g
​​​​​​Tap Density​​​:≥0.7g/cm³
D10​​:4.0±0.2μm
D50​:8.0±2μm
​​D90​:​​13.0±2.0μm
MOQ:10g
Leading time: 5-8 working days

Lithium-Rich Manganese-Based Polycrystalline Cathode Material SF-HV-LRM-1

​​Model:SF-HV-LRM-1
​​​​​​​Specific Surface Area​:3.6226m²/g
​​​​​​Tap Density​​​:2.1g/cm³
Discharge Capacity (2.0-4.8V):>300 (0.1C), 250 (1C)mAh/g
Initial Efficiency​:85%
​​Voltage Drop per Cycle​:​​0.6 (after 500 cycles)mV
​​Capacity Retention​:​​85 (after 500 cycles)%
MOQ:5pcs
Leading time: 5-8 working days

NCM811 Cathode Material MS-811-83 Single Crystal Lithium Niobate Coated

​​Model:MS-811-83
​​​​​​​Product Usage​:Laboratory
​​​​​​Calendering Density​​​:3.53g/cm³
SSA (BET):0.58m²/g
Element Content:82.1%
Application:​​Solid-state battery
MOQ:5g
Leading time: 5-8 working days

Pre-Slotted 18650/21700 Battery Case Kit (Pre-Nickel-Plated Steel) with Insulation Gaskets & Explosion-Proof Cap

Model:18650/21700 case ket
​Style:Pre-Slotted
​​Surface Finish​​:Pre-nickel plated steel
​​Wall Thickness:0.2-0.3mm
MOQ:50pcs
Leading time: 5-8 working days

18650 Cylindrical Battery Steel Case + Explosion-Proof Cap + Upper & Lower Insulation Sheets — Cylindrical Battery Case Set

Model:18650/21700 case ket
Surface Finish​:Pre-nickel plated steel
Shell and Cover Material​​:Nitric acid nickel-plated A3 steel
​​Sealing O-ring and Washer Material:Nylon
Gasket:PET
​​Wall Thickness:0.2-0.3mm
MOQ:50pcs
Leading time: 5-8 working days

CMC B-1 Sodium Carboxymethyl Cellulose Thickener and binder for lithium-ion batteries

Model:CMC B-1
Appearance​:White or Milky White
Purity:99.80
​​Viscosity of 1% Aqueous Solution:4270
Degree of Substitution:0.90
​​pH Value:7.5
​​Moisture:4.2
MOQ:50pcs
Leading time: 5-8 working days